WeldEye® User guide. Welding Procedures. Version 54 · PDF fileWeldEye® User guide....
Transcript of WeldEye® User guide. Welding Procedures. Version 54 · PDF fileWeldEye® User guide....
WeldEye User guide. Welding Procedures. Version 54 Page 1 of 77
Copyright by Weldindustry AS
Table of content
7. Welding Procedures ................................................................................................... 2 7.1. Create documents ....................................................................................................... 3
7.1.1. Open a new document .................................................................................... 3 7.1.2. Save a procedure .......................................................................................... 12 7.1.3. Sketches ........................................................................................................ 13
7.1.3.1. Draw or upload a sketch ........................................................................... 14 7.1.3.2. Copy a sketch from the sketch library to a procedure .............................. 20 7.1.3.3. Insert a sketch from an existing procedure ............................................... 22 7.1.3.4. Copy sketch to clipboard .......................................................................... 24 7.1.3.5. Copy sketch to Sketch Library ................................................................. 25 7.1.3.6. Delete sketch from Sketch Library ........................................................... 26
7.1.4. Set a procedure to Inactive ........................................................................... 27 7.1.5. Set a procedure to Active ............................................................................. 27 7.1.6. Sign a procedure ........................................................................................... 28 7.1.7. Revise a procedure ....................................................................................... 30 7.1.8. Additional Pages .......................................................................................... 31
7.1.8.1. Add extra text ........................................................................................... 31 7.1.8.2. Add extra sketch ....................................................................................... 35 7.1.8.3. Add extra file ............................................................................................ 38 7.1.8.4. Delete additional page .............................................................................. 42
7.2. Search for procedures ............................................................................................... 45 7.2.1. Welding Procedure Surveys ......................................................................... 51
7.2.1.1. Set procedures to Inactive ........................................................................ 53 7.2.1.2. Set procedures to Active .......................................................................... 55 7.2.1.3. Delete Welding Procedures ...................................................................... 58
7.2.2. Printouts ....................................................................................................... 60 7.2.2.1. Print out of single Welding Procedure (front page) ................................. 60 7.2.2.2. Print out of Welding Procedure Survey ................................................... 62 7.2.2.3. Printout of one or several procedures (Batch print) ................................. 65
7.3. Lists .......................................................................................................................... 71 7.3.1. Create new WP List(s) ................................................................................. 71
7.3.1.1. Add Welding Procedures to WP List ....................................................... 73 7.3.1.2. Remove Welding Procedures from WP List ............................................ 76
WeldEye User guide. Welding Procedures. Version 54 Page 2 of 77
Copyright by Weldindustry AS
7. Welding Procedures
Introduction In this part of the User Guide, it will be described how to: - Create new documents - Revise existing documents - Use the sketch library - Use the sketch tool - Search for existing documents - Printout of documents and document packages
Currently supported document layouts are:
o EN ISO pWPS o EN ISO WPQR o EN ISO WPS o EN ISO WPT o EN ISO WI o ASME PQR o ASME WPS
WeldEye User guide. Welding Procedures. Version 54 Page 3 of 77
Copyright by Weldindustry AS
7.1. Create documents 7.1.1. Open a new document
From the left side menu 1. Click on the Welding Procedure button. 2. Click on New 3. Click on the wanted document layout. In this case pWPS.
WeldEye User guide. Welding Procedures. Version 54 Page 4 of 77
Copyright by Weldindustry AS
An empty document (in this case pWPS) will appear on your screen:
4
3
6 5
2 1
WeldEye User guide. Welding Procedures. Version 54 Page 5 of 77
Copyright by Weldindustry AS
In a New document, certain icons and buttons are visible. After saving the document, more icons and buttons will appear. Note that the fields pWPS no. and Prod. by (1 above) is mandatory (must be filled in) before you are able to save. In the document there are fields with and without drop-down menus. If a field is having a drop-down menu, this icon is showed to the right of the field. (2 above)
There are also Go to icons in the document. The Go to icon is shown to the right of the field. (3 above). If a document number is referred to in a field, the document will open in a new window when click on the Go to icon. The referred document must of course exist in WeldEye. The documents includes an area for sketches (4 above)
Explanation to the icons and buttons
Click her to save the document
The document is set to Active as default. Remove the tag by click on it. The document is then set to Inactive. Instead of deleting the document, you can set it to inactive. The document is still in the database and its possible to search for inactive documents.
Possibility to state if a document is PED approved or not. Empty check box means no, checked (marked) Check box means yes. In Welding Procedure search, you are able to search for PED approved procedures. If a procedure is PED approved or not will show in the survey named Heading.
The fields in the different documents are very much the same. The following describes the terms in a general manner.
pWPS no Insert the documents number in this field. Ref. If you need to insert any reference in the document, insert it here.
Date This field is not for editing. The date will automatically show when you save the document. Requires that you have inserted a date in the date field (5 above), and your signature in the signature field (6 above).
Rev. Insert the document revision number in this field. Prod. by Enter who made this document. What you type in to this field is
optional. Usually your Company name or the name of the person who make the document is entered.
WeldEye User guide. Welding Procedures. Version 54 Page 6 of 77
Copyright by Weldindustry AS
Client Insert the name of the Client. If the document is to be made in a more
general manner, you can for example assign it as a general document or an internal document.
Ref. standard Insert a reference to a standard. The procedure must fulfill the
requirements in the stated standard. Examples of standards to be filled in can be: EN ISO 15614-1, ASME IX, NORSOK M-601 etc.
Project Insert the name of the Project this procedure shall be used on. If the
document is to be made in a more general manner, you can for example assign it as a general document or an internal document.
Ref. spec. Possibility to insert a reference to a specification. Many clients have
additional welding requirements in a project specific specification. Several companies have their own internal specifications. If so, you can insert a reference to the specification(s) in this field.
Exam. body If the procedure is approved by, or tested by a third party, you can enter
the name of the examination body in this field. Location Insert your Company location. Usually the name of the location to the
company who welds the qualification test is inserted in this field. Ref. WP If you want to refer to another welding procedure, insert the WP name
in this field. You can refer to four different documents. The fields has Go to icons (3 above) to the right, which means that the referred document will open directly in a new window when you click on the icon. The referred document must exist in WeldEye to open.
Welding Process Insert the name of the welding process. Three processes for
each procedure are supplied. Shielding gas type Insert the name of the shielding gas for each welding process. Weaving (yes/no) State yes or no. If yes, state the width of the weaving. Purging gas type State the name of the purging gas, if any. Welding positions State the welding position(s) to be used for a qualification or to
be used in production. Joint type State what type(s) of joint the welding procedure applies for. Joint preparation Describe how to do the joint preparation.
WeldEye User guide. Welding Procedures. Version 54 Page 7 of 77
Copyright by Weldindustry AS
Cleaning method Describe how to clean the joint before welding Backing Describe if backing shall be / are used. If used, enter the type. Single/Double State if the procedure applies for single sided