Thin and high-pitch laser- etched mesh manufacturing and bulking "
description
Transcript of Thin and high-pitch laser- etched mesh manufacturing and bulking "
![Page 1: Thin and high-pitch laser- etched mesh manufacturing and bulking "](https://reader036.fdocuments.in/reader036/viewer/2022062501/568164da550346895dd7292d/html5/thumbnails/1.jpg)
Thin and high-pitch laser-etched mesh manufacturing and bulking"
(INFN Bari, CEA Saclay, CERN)
RD51 Common Projects
V. Berardi, P. Colas, Rui de Oliveira
![Page 2: Thin and high-pitch laser- etched mesh manufacturing and bulking "](https://reader036.fdocuments.in/reader036/viewer/2022062501/568164da550346895dd7292d/html5/thumbnails/2.jpg)
Motivation
• Thin foil (5 micron Cu for instance) to maximize the gain
• High pitch (>1000 lpi) to reduce ion backflow (see NIM A 535 (2004) 226)
As a conclusion it is expected that the optimal ion backflow conditions will be fulfilled with a 1000 lpi mesh for 100 micron gap, and with a 1500 lpi mesh for 50 micron:
![Page 3: Thin and high-pitch laser- etched mesh manufacturing and bulking "](https://reader036.fdocuments.in/reader036/viewer/2022062501/568164da550346895dd7292d/html5/thumbnails/3.jpg)
Bulking of thin meshesPresently ‘bulk’ Micromegas are made with woven meshes, 380-450 lpi.Let us try electroformed thin meshes
![Page 4: Thin and high-pitch laser- etched mesh manufacturing and bulking "](https://reader036.fdocuments.in/reader036/viewer/2022062501/568164da550346895dd7292d/html5/thumbnails/4.jpg)
Ultrafast laser drilling
10/10/2010 RD51 Bari WG1 4
• New high-rate ‘fs’ lasers make it possible to drill more perfect holes (no melting) in quantities.
• Might replace wet etching for some materials (ceramics) or down to 10 µ diameter
fs ps ns µs
Various processes at various time scales
Laser trepanned hole
![Page 5: Thin and high-pitch laser- etched mesh manufacturing and bulking "](https://reader036.fdocuments.in/reader036/viewer/2022062501/568164da550346895dd7292d/html5/thumbnails/5.jpg)
Fori Cu 20x20_50ms_500mW_inf_50x Fori Cu 20x20_50ms_500mW_50x
Fori 50ms_700mW_50x
![Page 6: Thin and high-pitch laser- etched mesh manufacturing and bulking "](https://reader036.fdocuments.in/reader036/viewer/2022062501/568164da550346895dd7292d/html5/thumbnails/6.jpg)
![Page 7: Thin and high-pitch laser- etched mesh manufacturing and bulking "](https://reader036.fdocuments.in/reader036/viewer/2022062501/568164da550346895dd7292d/html5/thumbnails/7.jpg)
Duration, Milestones and Funding
• The project is for an initial duration of 1 year, starting Feb. 15, 2012
• There will be presentations in every collaboration meeting (mid-June and early October)
• The tasks will be shared as follows: – Bari : improve laser punching technique– CEA Saclay : test of meshes, gain ion back-flow– CERN: bulking with various meshes
• Funding: 19 000 CHF (8 000 Bari, 5000 Saclay, 6000 CERN)