![Page 1: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/1.jpg)
KARNATAK LAW SOCIETY‟S
GOGTE INSTITUTE OF TECHNOLOGY
UDYAMBAG, BELAGAVI-590008
(An Autonomous Institution under Visvesvaraya Technological University, Belagavi)
(APPROVED BY AICTE, NEW DELHI)
Department of Mechanical Engineering
Scheme and Syllabus (2016 Scheme)
2nd
Semester Computer Integrated Manufacturing
![Page 2: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/2.jpg)
INSTITUTION VISION
Gogte Institute of Technology shall stand out as an institution of excellence in technical education and
in training individuals for outstanding caliber, character coupled with creativity and entrepreneurial
skills.
MISSION
To train the students to become Quality Engineers with High Standards of Professionalism and Ethics
who have Positive Attitude, a Perfect blend of Techno-Managerial Skills and Problem solving ability
with an analytical and innovative mindset.
QUALITY POLICY
Imparting value added technical education with state-of-the-art technology in a congenial,
disciplined and a research oriented environment.
Fostering cultural, ethical, moral and social values in the human resources of the institution.
Reinforcing our bonds with the Parents, Industry, Alumni, and to seek their suggestions for
innovating and excelling in every sphere of quality education.
DEPARTMENT VISION
To emerge as a center of excellence in technical education and research by moulding students with techno managerial skills coupled with ethics and to cater to the needs of the industry and society in
general.
MISSION
To impart value based education and to promote research and training in frontier areas to face the
challenges in the changing global scenario; to provide impetus to industry institute relation, to imbibe
social, ethical, managerial and entrepreneurial values in students.
PROGRAM EDUCATIONAL OBJECTIVES (PEOs)
1.
The graduates will acquire core competence in basic science and mechanical engineering
fundamentals necessary to formulate, analyze and solve engineering problems and to pursue
advanced study or research.
2. The graduates will engage in the activities that demonstrate desire for ongoing personal and
professional growth and self-confidence to adapt to rapid and major changes.
3.
The graduates will maintain high professionalism and ethical standards, effective oral and written communication skills, work as part of teams on multi-disciplinary projects under diverse
professional environments and relate engineering issues to the society, global economy and to
emerging technologies.
![Page 3: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/3.jpg)
PROGRAM OUTCOMES (POs)
1. Scholarship of Knowledge:
Graduates shall acquire in-depth knowledge in machine design and update the same, integrating existing and updated knowledge in global perspective.
2. Critical Thinking:
Graduates shall possess ability for independent judgement based on critical analysis and also for synthesis of information for extensive research in the area of specialization.
3. Problem Solving:
Graduates shall conceptualize through lateral thinking and obtain feasible and optimal solutions
for engineering problems considering societal and environmental requirements. 4. Research Skill:
Graduates shall review relevant literature, apply appropriate research methodologies, working
individually or as a team contributing to the advancement of domain knowledge 5. Usage of modern tools:
Graduates shall be able to adopt modern techniques, analytical tools and softwares for complex
engineering solutions. 6. Collaborative and Multidisciplinary work:
Graduates shall be able to engage in collaborative multidisciplinary scientific research for
decision making through rational analysis.
7. Project Management and Finance: Graduates shall be able to apply engineering and management principles for efficient project
management considering economical and financial factors.
8. Communication: Graduates shall possess communication skills to comprehend, document and present effectively
to the engineering community and society at large.
9. Life-long Learning: Graduates shall engage in lifelong learning with motivation and commitment for professional
advancement.
10. Ethical Practices and Social Responsibility:
Graduates shall imbibe the professional ethics and integrity for sustainable development of society.
11. Independent and Reflective Learning:
Graduate shall be able to introspect and apply corrections.
![Page 4: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/4.jpg)
Scheme of Teaching for M. Tech. Computer Integrated Manufacturing CIM (2016-17)
Curriculum frame work: Department of Mechanical Engineering
S.No. Subject Area Credits
1 Professional Core ( Theory & Practical) PC 36
2 Professional Elective PE 16
3 Lab PC 4
4 Seminar PC 2
5 Internship SS 10
6 Project PR 22
7 Term assignment 4
Total 94
Lecture (L):One Hour /week – 1 credit
Practical (P): Two hours /week – 1 credit
Distribution of credits
Semester Credits
1 25
2 25
3 26
4 18
Total 94
![Page 5: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/5.jpg)
SEE: SEE (Theory exam) will be conducted for 100marks of 3 hours duration. It is reduced to 50
marks for the calculation of SGPA and CGPA
Term Assignment: The performance is continuously evaluated by the faculty member and Grade
is given.
Elective – B
CIM251 Advanced Tool EngineeringDesign
CIM252 Non DestructiveTesting CIM253 Artificial Intelligence and ExpertSystems
CIM254 Advanced ControlEngineering
Second Semester
S.
No.
Subject
Code Subject
Credits Total
credits
Contact
Hours/
week
Marks
L – T - P CIE SE
E
TOTA
L
1. CIM21 Advanced Foundry
Technology PC 4-0 -0 4 4 50 50 100
2. CIM22 Industrial Robotics PC 4-0 -0 4 4 50 50 100
3. CIM23 Non Traditional
Machining PC 4-0 -0 4 4 50 50 100
4. CIM24
Flexible
Manufacturing
Systems
PC 4 -0 -0 4 4 50 50 100
5. CIM25X Elective-B PE 4 - 0 -0 4 4 50 50 100
6. CIM26
Rapid Prototyping
and Casting
Analysis Lab
PC 0 – 0 - 2 2 3 25 25 50
7. CIM27 Seminar-2 PC 1 - 0-1 1 25 25
8. PTA28 Mini Project-2 0 – 0 - 2 2 4 25 25
Total 25 30 300 300 600
![Page 6: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/6.jpg)
ADVANCED FOUNDRY TECHNOLOGY
Course Code CIM21 Credits 4
Course type PC CIE Marks 50 marks
Hours/week: L-T-P 4-0-0 SEE Marks 50 marks
Total Hours: 50 SEE Duration 3 Hours for 100 marks
Course learning objectives
1. Foundry metallurgy and concept of solidification of metals. Interpretation and use of cooling curves.
2. Design principles of Casting, Gating and Riser system.
3. Advanced melting techniques and quality control of castings. 4. Cast iron foundry, particular attention to grey cast iron, ductile iron and malleable iron.
5. Aluminum alloy foundry practice discussing principal alloys such as Al-Si, Al-Cu and Al-Zn-
Mg. 6. Automation and Modernization of foundry. Robotic applications.
Pre-requisites :Basic Knowledge of Foundry technology and material science
Unit – I 10 Hours
FoundryMetallurgy:Oxidation of liquid metals, gas dissolution in liquid metals, methods of
degassing, fluidity, factors affecting fluidity, fluidity tests, hot tearing, Shrinkage of liquid
metals.Solidification of Casting: Concept of solidification of metals. Homogenous and heterogeneous
nucleation. Growth mechanism. Solidification of pure metals and alloys. Mechanism of columnar and
dendritic growth. Coring or Segregation. Solidification time and Chvorinov‟s rule. Concept of progressive and directional solidification. Interpretation and Use of Cooling Curves(Thermal
Analysis), X-Ray Imaging of Solidification Processes and Microstructure Evolution
Unit – II 10 Hours
Casting Design: Initial considerations in design, Functional design, Simplification of foundry practices, Metallurgical design, Economic considerations.
Riser Design: Types of risers and their application, Optimum riser design, Feed metal volume, Riser
location, Progressive and directional Solidification, Feeding Distance, NRL method, Feeding aids used in riser design, Factors in riser size, computerized method of riser design.
Gating Design: Components of Gating system, Effects of gates on aspiration, turbulence and dross
trap, Pressurized versus unpressurized systems, Vertical versus horizontal gating systems.
Unit - III 10 Hours Furnace Technology: Cupola and its recent developments, charge calculation, Electron Beam
Melting, Plasma Melting and Heating, Electro slag, Re melting.
Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects, Gas defects, Shrinkage defects, Contraction defects,
Dimensional errors, Compositional errors and segregation. Different inspection and testing methods
to evaluate the casting. Coating of Castings, Quality control activities in a foundry
![Page 7: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/7.jpg)
Unit - IV 10 Hours
Grey cast iron foundry practice: Melting practice, Inoculation, grey iron alloying, pouring, Gating and feeding systems, Foundry properties and engineering properties, Specification, Heat treatment,
Applications.
Ductile iron foundry practice: Melting practice, Desulfurization methods, Composition control, magnesium treatment, inoculation, casting and solidification, Engineering Properties, Austempered
Ductile iron(ADI),Applications.
Malleable iron foundry practice: Melting practice, Structure of White-heart and black-heart malleable
cast iron, Pearlitic malleable iron, Properties and applications. Cast Iron Metallurgy
Classification of cast iron, Composition and graphitization, Carbon equivalent, Graphite morphology,
effect of various elements. Special casting processes Investment casting, Die casting, centrifugal casting, full mould casting, vacuum shield casting etc
Unit - V 10 Hours
Soft Material foundry Practice: Aluminum casting-Composition, properties and application of
common aluminum alloy casting, Melting and casting of aluminum alloys, Gating and risering of Al-alloy casting, Copper alloy foundry practice- General characteristics of common cast copper alloys,
Melting and casting of copper alloys, Gating and risering of copper alloy castings.
Foundry Automation and Modernization: Introduction to modernization. Mechanization of foundry and its advantages. Mechanization of sand plant, moulding and core making mechanization in
melting, pouring and shake out units. Material handling equipments and conveyor systems. Foundry
robotic applications.
Books
1. R W Heine,C R Loper, and P C Rosenthal, Principles of Metal Casting, Tata McGraw Hill,
1976 2. P.R. Beelely, Foundry Technology, Butterworth ,2001
3. Titov Stepnov, Foundries practice
4. M.Lal and O.P. Khanna, A Text Book of Foundry Technology, Dhanpat Rai & Sons ,2007
5. ASM Handbook, Casting, Vol. 15, ASM Publication, Materials Park, Ohio,2008. 6. Hans Roedter, The Essential of Gating and Risering system Design, Rio Tinto Iron and
Titanium Inc.2000
7 P.C. Mukherjee, Fundamentals of Metal casting Technology
8 P.D.Webster, Fundamentals of Foundry Technology
Course Outcome (COs)
At the end of the course, the student will be able to Bloom‟s
Level
1. Design casting, gating and risering systems [L6]
2.
The students will get a clear thought on importance of solidification of advanced
alloys, interpretation of cooling curves, imaging of solidification process and
microstructure evaluation [L3]
3. The student will recognize the different types of melting and molding techniques
for a particular alloy [L2]
4. They will be able to appraise control casting quality, knowledge in inspection, testing methods and statistical quality control activities
[L5]
5. Ability to use the methods, skills and engineering tools to produce castings of grey
cast iron, ductile iron and malleable iron [L3]
6 Develop foundry practice for advanced soft materials [L6] 7 Ability to implement computer and robot technology in the foundry process to [L5]
![Page 8: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/8.jpg)
meet desired needs and to function on multi disciplinary team
8 Broad education to understand the impact of mechanization in melting, pouring and material handling
[L2]
Program Outcome of this course (POs) PO No.
1. Graduates shall acquire in-depth knowledge in machine design and update the same,
integrating existing and updated knowledge in global perspective. [PO1]
2. Graduates shall possess ability for independent judgment based on critical analysis and also for synthesis of information for extensive research in the area of
specialization. [PO2]
3.
Graduates shall conceptualize through lateral thinking and obtain feasible and
optimal solutions for engineering problems considering societal and environmental
requirements
[PO3]
Course delivery methods Assessment methods
1. Black Board Teaching 1. Internal Assessment
2. Power Point Presentation 2. Assignment
3. Working Models 3. Seminar
4. Videos 4. Mini-project
Scheme of Continuous Internal Evaluation (CIE):
Components Average of best two IA
tests out of three
Average of
assignments (Two) / activity
Seminar/Mini
Project
Total
Marks
Maximum Marks: 50 30 10 10 50
Self Study topics shall be evaluated during CIE (Assignments and IA tests) and 10% weightage
shall be given in SEE question paper.
Scheme of Semester End Examination (SEE):
1. It will be conducted for 100 marks of 3 hours duration. It will be reduced to 50 marks for the
calculation of SGPA and CGPA.
2. Minimum marks required in SEE to pass: 20
3. Question paper contains 08 questions each carrying 20 marks. Students have to answer FIVE full
questions. SEE question paper will have two compulsory questions (any 2 units) and choice will
be given in the remaining three units.
![Page 9: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/9.jpg)
INDUSTIRAL ROBOTICS
Course Code CIM22 Credits 4
Course type PC CIE Marks 50 marks
Hours/week: L-T-P 4-0-0 SEE Marks 50 marks
Total Hours: 50 SEE Duration 3 Hours for 100 marks
Course learning objectives
1. To introduce the basic concepts, parts of robots and types of robots. 2. To study different robot transformations and sensors.
3. To study the kinematics and dynamics of different standard configuration of manipulators.
4. To make the student familiar with the various drive systems for robot, sensors and their
applications in robots. 5. To understand various control systems and their applications in robot
Pre-requisites :Basic knowledge of mathematics- matrices, control systems.
Unit – I 10 Hours
Introduction: Automation and Robotics, Historical Development, Definitions, Basic Structure of
Robots, Robot Anatomy, Complete Classification of Robots, Fundamentals about Robot Technology,
Factors related to use Robot Performance, Basic Robot Configurations and their Relative Merits and
Demerits, Types of Drive Systems and their Relative Merits, the Wrist & Gripper Subassemblies.
ROBOT TRANSFORMATIONS: 2D and 3D Transformation-Scaling, Rotation, Translation-
Homogeneous coordinates, multiple transformation-Simple problems.
Self learning topics: Automation and Robotics, Historical Development, Definitions, Basic Structure of Robots, Robot Anatomy, Complete Classification of Robots, Fundamentals about Robot
Technology, Factors related to use Robot Performance, Basic Robot Configurations and their Relative
Merits and Demerits
Unit – II 10 Hours Kinematics of Robot Manipulator: Introduction, General Description of Robot Manipulator,
Homogenous Representation of Objects, Robotic Manipulator Joint Co-Ordinate System, Euler
Angle & Euler Transformations, Roll-Pitch-Yaw(RPY) Transformation, Direct & Inverse
Kinematics Solution, D H Representation & Displacement Matrices for Standard Configurations.
Unit – III 10 Hours
Dynamics of Robotic Manipulators: Introduction, Brief Discussion on Lagrange–Euler (LE)
Dynamic Modeling of Robotic Manipulators: - Preliminary Definitions, Generalized Robotic Coordinates, Dynamic Constraints, Newton‟s Equation, Euler Equation, The Lagrangian & Lagrange‟s
Equations. Applications of Lagrange– Euler (LE), Dynamic Modeling of Robotic Manipulators: -
Velocity of Joints, Kinetic Energy of Arm, Potential Energy of Robotic Arm, The Lagrange of two Link Robotic Dynamics with Distributed Mass
Unit – IV 10 Hours
Robotic Motion Trajectory Design: – Introduction, Trajectory Interpolators, Basic Structure of
Trajectory Interpolators, Cubic Joint Trajectories. General Design Consideration on Trajectories:-4-
3-4 & 3-5-3 trajectories.
![Page 10: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/10.jpg)
Robot Teaching: Introduction, Various Teaching Methods, Task Programming, Survey of Robot
Level Programming Languages, WAIT, SIGNAL & DELAY Commands, various Textual Robot
Languages Such as VAL II, RAIL, AML and their Features, Typical Programming Examples such as
Palletizing, Loading Etc.
Unit – V 10 Hours
Robot Sensing & Vision: Various Sensors and their Classification, Use of Sensors and Sensor Based
System in Robotics, Machine Vision System, Description, Sensing, Digitizing, Image Processing and
Analysis and Application of Machine Vision System.
Industrial Applications: Objectives, Automation in Manufacturing, Robot Application in Industry,
Task Programming, Goals of AI Research, AI Techniques.
Self learning topics: Objectives, Automation in Manufacturing, Robot Application in Industry, Task Programming, Goals of AI Research, AI Techniques.
Books 1. Mohsen Shahinpoor, A Robot Engineering Textbook, Harper & Row publishers, New York,
1987
2. S. B. Niku, Introduction to Robotics Analysis, Systems, Applications, Pearson Education,
2008.
3. Fu, Lee and Gonzalez, Robotics, control vision and intelligence, McGraw Hill International,
1987.
4. J. J. Craig, Introduction to Robotics: Mechanical and Control, Addison-Wesley, 2nd
Ed.1989 5. R. J. Schilling, Fundamentals of Robotics, Analysis and Control, PHI, 2006
6. Yoram Koren, Robotics for Engineers, McGraw Hill International, 1985
7. Groover, Weiss, Nagel, Industrial Robotics, McGraw Hill International, 1986 8. Keramas, Thomson, Robot Technology Fundaments, Vikas Publication House, 1999.
9 Klafter, Chmielewski and Negin, Robotic engineering - An Integrated approach, PHI, 1989.
10 Mikell. P. Groover, Industrial Robotics Technology-Programming and Applications, McGraw Hill Co, 1995
Course Outcome (COs)
At the end of the course, the student will be able to Bloom‟s
Level
1. Familiarize with the history, concept development and key components of robotics
technologies [L2]
2. Understand basic mathematic manipulations of spatial coordinate representation
and transformation [L2, L4]
3. Understand and able to solve basic robot forward and inverse kinematics problems [L2,L3]
4. Understand and able to solve basic robotic dynamics, path planning and control
problems [L2,L3]
5. Understand and demonstrate principles of various Sensors and their applications in
robots [L2]
![Page 11: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/11.jpg)
Program Outcome of this course (POs) PO No.
1. Graduates shall possess ability for independent judgement based on critical analysis and also for synthesis of information for extensive research in the area of
specialization. [PO2]
2. Graduates shall conceptualise through lateral thinking and obtain feasible and optimal solutions for engineering problems considering societal and environmental
requirements
[PO3]
3.
Graduates shall review relevant literature, apply appropriate research methodologies,
working individually or as a team contributing to the advancement of domain knowledge.
[PO4]
4. Graduates shall be able to adopt modern techniques, analytical tools and softwares
for complex engineering solutions. [PO5]
Course delivery methods Assessment methods
1. Black Board Teaching 1. Internal Assessment
2. Power Point Presentation 2. Assignment
3. Working Models 3. Seminar
4. Videos 4. Mini-project
Scheme of Continuous Internal Evaluation (CIE):
Components Average of best two
IA tests out of three
Average of
assignments (Two) /
activity
Seminar/Mini
Project
Total Marks
Maximum Marks: 50 30 10 10 50
Self Study topics shall be evaluated during CIE (Assignments and IA tests) and 10% weightage
shall be given in SEE question paper.
Scheme of Semester End Examination (SEE):
1. It will be conducted for 100 marks of 3 hours duration. It will be reduced to 50 marks for the
calculation of SGPA and CGPA.
2. Minimum marks required in SEE to pass: 20
3. Question paper contains 08 questions each carrying 20 marks. Students have to answer FIVE full
questions. SEE question paper will have two compulsory questions (any 2 units) and choice will
be given in the remaining three units.
![Page 12: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/12.jpg)
NON TRADITIONAL MACHINING
Course Code CIM23 Credits 4
Course type PC CIE Marks 50 marks
Hours/week: L-T-P 4-0-0 SEE Marks 50 marks
Total Hours: 50 SEE Duration 3 Hours for 100 marks
Course learning objectives
1. To introduce the concept of non-traditional machining (NTM) processes and the need/scope of those processes.
2. To present an overview of classification and comparison between conventional and non-
conventional machining process 3. To lay a firm foundation with regard to the principles, equipments and applications of NTM
processes with emphasis on the latest developments.
4. To analyze some of the NTM processes with regard to the material removal rate (mrr) and to solve related engineering problems.
Pre-requisites :Basic knowledge of Conventional manufacturing and its concepts.
Unit - I 10 Hours Introduction: History, Classification, comparison between conventional and Non- conventional
machining, process selection.
Ultrasonic Machining (USM): Introduction, equipment, tool materials & tool size, abrasive slurry,
Acoustic Head, Tool Feed Mechanisms, Mechanics of USM, Expression for MRR:- Effect of
process parameters: Effect of amplitude and frequency and vibration, Effect of abrasive grain
diameter, effect of applied static load, effect of slurry concentration, tool & work material, USM
process characteristics: Material removal rate, tool wear, Accuracy, surface finish, Numerical
Problems
Self learning topics:applications, advantages & Disadvantages of USM, Latest Developments
Unit - II 10 Hours
Abrasive Jet Machining (AJM): Introduction, Equipment, Variables in AJM: Carrier Gas, Type of
abrasive, size of abrasive grain, velocity of the abrasive jet, mean number, abrasive particles per
unit volume of the carrier gas, work material, stand- off distance (SOD), nozzle design, shape of
cut. Process characteristics-Material removal rate, Nozzle wear, Accuracy & surface finish.
Applications, advantages & Disadvantages of AJM. Water Jet Machining (WJM): Principal,
Equipment, Operation, Application.
Self Learning Topics: Advantages and limitations of water Jet machining, Abrasive water Jet
machining, Latest Developments in AJM, WJM
Unit - III 10 Hours
Electrochemical Machining (ECM): Introduction, study of ECM machine, elements of ECM process
: Cathode tool, Anode work piece, source of DC power, Electrolyte, chemistry of the process, ECM
Process characteristics – Material removal rate, Kinematics and Dynamics of ECM, Accuracy, surface
finish, Selective Dissolution, Effect of Heat and Hydrogen Gas Bubbles, ECM Tooling: ECM tooling
technique & example, Tool & insulation materials, Tool size Electrolyte flow arrangement, Handling
of slug, Economics of ECM, Applications such as Electrochemical turning, Electrochemical Grinding,
![Page 13: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/13.jpg)
Advantages, Limitations. Numerical Problems, Latest Developments.
Chemical Machining (CHM): Introduction, elements of process, chemical blanking process :
Preparation of work piece, preparation of masters, masking with photo resists, etching for blanking,
accuracy of chemical blanking, applications of chemical blanking, chemical milling (contour
machining): process steps –masking, Etching, process characteristics of CHM: material removal rate,
accuracy, surface finish, advantages & application of CHM. Latest Developments.
Self Learning Topics: Electrochemical Honing, Electrochemical De-burring, Hydrogen
embrittlement
Unit - IV 10 Hours
Electrical Discharge Machining (EDM): Introduction, mechanism of metal removal, EDM Circuits and Operating Principles, dielectric fluid, spark generator, EDM tools (electrodes) Electrode feed
control, Electrode manufacture, Electrode wear, EDM tool design, choice of machining operation,
electrode material selection, under sizing and length of electrode, machining time. Flushing; pressure flushing, suction flushing, side flushing, pulsed flushing synchronized with electrode movement, EDM
process characteristics: metal removal rate, accuracy, surface finish, Machining Accuracy, Heat
Affected Zone. Machine tool selection, Application, EDM accessories / applications, electrical discharge grinding. Numerical Problems.
Self Learning Topics: traveling wire EDM, Latest Developments
Unit - V 10 Hours Plasma Arc Machining (PAM): Introduction, equipment, non-thermal generation of plasma,
selection of gas, Mechanism of metal removal, PAM parameters, process characteristics, PAM Torch,
Accuracy and Surface Finish, Metallurgical Effects, Safety precautions, Latest Developments.
Laser Beam Machining (LBM): Introduction, equipment of LBM mechanism of metal removal,
LBM parameters, Process characteristics. Numerical Problems, Latest Developments.
Electron Beam Machining (EBM): Principles, Mechanics of EBM equipment, operations. Numerical
Problems, Latest Developments.
Self Learning Topics: applications, advantages and limitation of PAM, EBM and LBM.
Books 1. Pandey and Shan, Modern Machining Process, Tata McGraw Hill, 2000. 2. Amitabha Ghosh and Asok Kumar Mallik, Manufacturing Science, Affiliated East-West
Press Pvt. Ltd., New Delhi, 2010. 3. 1. HMT, Production Technology, Tata McGraw Hill, 2001
4. 2. P.K.Mishra, Non-Conventional Machining, The Institution of Engineers (India) Test
book series, Narosa Publishing House, 2005.
5. 3. NPTEL Notes nptel.ac.in/downloads/
Course Outcome (COs)
At the end of the course, the student will be able to Bloom‟s
Level
1. Explain the concept and evolution of Non -Traditional Machining (NTM)
processes. [L2]
2. Explain equipment, mechanism of material removal and effect of different process parameters in the mechanical NTM processes (AJM, USM, WJM) and thermal
NTM processes (EDM, PAM, LBM, EBM) [L3, L4]
3. Explain equipment, mechanism of material removal and effect of different [L6]
![Page 14: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/14.jpg)
process parameters in the chemical and electrochemical NTM processes (CHM,
ECM) [L3, L4]
4. Solve numerical problems and explain latest developments related to NTM
processes. [L4]
Program Outcome of this course (POs) PO No.
1. Graduates shall acquire in-depth knowledge in machine design and update the same, integrating existing and updated knowledge in global perspective.
[PO1]
3.
Graduates shall conceptualise through lateral thinking and obtain feasible and
optimal solutions for engineering problems considering societal and environmental
requirements. [PO3]
3. Graduates shall be able to adopt modern techniques, analytical tools and softwares
for complex engineering solutions [PO5]
Course delivery methods Assessment methods
1. Black Board Teaching 1. Internal Assessment
2. Power Point Presentation 2. Assignment
3. Working Models 3. Seminar
4. Videos 4. Mini-project
Scheme of Continuous Internal Evaluation (CIE):
Components Average of best two IA
tests out of three
Average of
assignments (Two) / activity
Seminar/Mini
Project
Total
Marks
Maximum Marks: 50 30 10 10 50
Self Study topics shall be evaluated during CIE (Assignments and IA tests) and 10% weightage
shall be given in SEE question paper.
Scheme of Semester End Examination (SEE):
1. It will be conducted for 100 marks of 3 hours duration. It will be reduced to 50 marks for the
calculation of SGPA and CGPA.
2. Minimum marks required in SEE to pass: 20
3. Question paper contains 08 questions each carrying 20 marks. Students have to answer FIVE full
questions. SEE question paper will have two compulsory questions (any 2 units) and choice will
be given in the remaining three units.
![Page 15: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/15.jpg)
FLEXIBLE MANUFACTURING SYSTEMS
Course Code CIM24 Credits 4
Course type PC CIE Marks 50 marks
Hours/week: L-T-P 4-0-0 SEE Marks 50 marks
Total Hours: 50 SEE Duration 3 Hours for 100 marks
Course learning objectives
1. To impart the concept & need for flexibility in manufacturing industries. 2. To impart the knowledge required to develop and implement an FMS.
3. To study the different types of automated material transport systems its design and analysis for
different applications both AS/RS and Carousel storage system. 4. To understand the concepts of group technology and cellular manufacturing.
5. To learn the perception of aggregate production planning, master production schedule,
MRP and Inventory control.
Pre-requisites :Basics of manufacturing processes and computer integrated manufacturing.
Unit – I 10 Hours
Definition of an FMS: Types, configurations & concepts – Types of flexibility & performance
measures. Function of FMS host computer, FMS host and area controller function distribution. Development and implementation of an FMS: Planning phase, Integration, System configuration,
FMS layouts, Simulation, FMS Project development steps.
Self Learning Topics: Project management, Equipment development, Host system development, planning, and Hardware & Software development.
Unit – II 10 Hours Automated Material Handling & Storages systems: Functions, Types, Analysis of material handling
equipments, Design of Conveyor & AGV systems. Benefits of Automated material handling
systems. Problems. Storage system performance, AS/RS, Carousel storage system, WIP storage system
Unit – III 10 Hours Group Technology and Cellular Manufacturing: Introduction, Part families, parts classification and
coding, production flow analysis, Machine cell design, Benefits of Group Technology.
Quality programs for manufacturing: Quality in design and manufacturing, Traditional and Modern quality control, Process variability Process Capabilty , SPC and Six sigma.
Unit – IV 10 Hours
Production Planning & Control system : Aggregate production planning and master production
schedule, material requirement planning, Just-In-Time : Definition JIT, Concept, Objectives
Self learning topics: Capacity planning, shop floor control, Inventory control, Extension of MRP.
Unit – V 10 Hours Scheduling: Introduction, Scheduling of operations on a single machine, 2 machine flow shop
scheduling, 2 machine job shop scheduling, 3 machine flow shop scheduling, scheduling „n‟
operations on „n‟ machines, Scheduling rules, loading problems , Tool management of FMS, material Handling system schedule. Problems.
![Page 16: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/16.jpg)
Books
1. M.P. Groover, Production Systems and Computer Integrated Manufacturing, Automation, Prentice Hall India (P) Ltd, 2008.
2. D J Parrish, Butter Worth , Flexible manufacturing – Heinemann, Ltd Oxford, 1993. 3. William W. Luggen, Flexible Manufacturing Cells & Systems –Prentice hall, NJ.
4. D M Considine, and G D Considine, Standard Handbook of Industrial Automation -Chopman and Hall, London, 1986.
Course Outcome (COs)
At the end of the course, the student will be able to Bloom‟s
Level
1. Students will learn and understand the concepts, techniques and applications of
flexible Manufacturing System [L2]
2. The students will be able to describe an FMS system in present manufacturing
scenario [L2]
3. The student will understand the different types of FMS layouts, material transport
and retrieval systems [L2]
4. To solve the sequencing problems for different cases and tool management [L2]
Program Outcome of this course (POs) PO No.
1. Graduates shall acquire in-depth knowledge in machine design and update the same,
integrating existing and updated knowledge in global perspective. [PO1]
2. Graduates shall be able to adopt modern techniques, analytical tools and softwares for complex engineering solutions
[PO5]
3. Graduates shall possess communication skills to comprehend, document and present
effectively to the engineering community and society at large. [PO8]
Course delivery methods Assessment methods
1. Black Board Teaching 1. Internal Assessment
2. Power Point Presentation 2. Assignment
3. Working Models 3. Seminar
4. Videos 4. Mini-project
Scheme of Continuous Internal Evaluation (CIE):
Components Average of best two
IA tests out of three
Average of
assignments (Two) / activity
Seminar/Mini
Project
Total
Marks
Maximum Marks: 50 30 10 10 50
Self Study topics shall be evaluated during CIE (Assignments and IA tests) and 10% weightage
shall be given in SEE question paper.
Scheme of Semester End Examination (SEE):
1. It will be conducted for 100 marks of 3 hours duration. It will be reduced to 50 marks for the
calculation of SGPA and CGPA.
2. Minimum marks required in SEE to pass: 20
![Page 17: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/17.jpg)
3. Question paper contains 08 questions each carrying 20 marks. Students have to answer FIVE full
questions. SEE question paper will have two compulsory questions (any 2 units) and choice will
be given in the remaining three units.
![Page 18: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/18.jpg)
ADVANCED TOOL DESIGN
Course Code CIM251 Credits 4
Course type PE CIE Marks 50 marks
Hours/week: L-T-P 4-0-0 SEE Marks 50 marks
Total Hours: 50 SEE Duration 3 Hours for 100 marks
Course learning objectives
1. To impart the basic concepts and fundamentals of Tool engineering, its techniques and applications
2. To comprehend the relationship between Tool s and Machine tool
3. To enhance awareness in the recent aspects of Tool engineering.
Pre-requisites :Basic Knowledge of machine tools and cutting tools and also machining process.
Unit - I 10 Hours
Introduction to tool design of Single point Cutting Tools
Introduction to tool design: Tooling, requirements of a tool designer, general tool design
procedure. Design of Single point Cutting Tools. Design of single point lathe tool. Design of
shank dimension using strength and rigidity considerations for rectangular, square and round cross
section and selection of tool geometry.
Self Learning Topics: Solid type tool, brazed tip tool, long indexable insert, throwaway index
able insert types and chip breakers.
Unit - II 10 Hours
Design of Multi Point Cutting Tool
Design of milling cutter. Design of elements like number of teeth and height circular pitch, body
thickness, chamfer width, fillet radius and selection of tool geometry.
Self Learning Topics: Drill bit design of elements like back taper, web thickness, land width,
margin, flute length and cross section and selection of tool geometry.
Unit - III 10 Hours
Design of Jigs and Fixtures
Functions and differences between jigs and fixtures ,advantages in mass production, design
principles, economics of jigs and fixtures. Principles of location -3-2-1 and 4-1-1 types of
locations, different types of locating elements. Clamping – Principles of clamping, types of
clamping including power clamping devices. Drill jigs- Types, Drill bushes, simple exercises of designing jigs for given components. Fixture Design turning fixtures, milling fixtures, grinding
and broaching fixtures, indexing fixtures. Design of fixtures for simple components.
Unit - IV
10 Hours
Design of Sheet Metal
Working of a power press and classification of presses. Components of a simple die, press tool
operation, die accessories, shearing action in punch & die, clearance ,shear on punch and die, Centre
of pressure and problems, scrap strip layout. Simple, progressive, compound, combination and
![Page 19: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/19.jpg)
inverted dies. Design problems on blanking and piercing dies for simple components.
Injection Molding
Injection moulding machine and its elements, general configuration of a mould. 2 plate and 3 plate mould. Introduction, to gate, runner, parting surface, ejection system. Core and cooling system.
Introduction to compression, transfer, blow moulding, extrusion, forming and calendaring.
Unit - V 10 Hours
Die Casting Dies Terminology: Core, cavity, sprue, slug, fixed and movable cores, finger cams, draft, and ejector pins ejector plates, gate, goose nozzle, over-flow, platten, plunger, runner, vent, water-line etc. Types of
Dies: Single cavity, multicavity dies, combination dies, unit dies, advantages and disadvantages of
types of dies. Die casting dies, unit dies. Advantages and disadvantages of types of dies. Die casting alloys, defects in die casting, finishing trimming and inspection of die casting components, safety,
and modern trends in die casting dies.
Books
1. C. Donaldson, G.H.LeCain ,V.C.Goold , Tool Design, Tata McGraw Hill pub.1976 2. M.H.A Kempster, Introduction to Jigs and Fixture Design ,Elbs Edition1974
3. P.N.Rao, Manufacturing Technology (Foundry, Forming and Welding) Tata Mcgraw Hill Publication Edition1996.
4. RGW Pye John, Injection Moulding Design,1998
5. D. V. Rosato& Donald V. Rosato Injection Moulding Handbook, CBS Publishers 1996
Course Outcome (COs)
At the end of the course, the student will be able to Bloom‟s
Level
1. Students will learn the concepts, techniques and applications of Tool Design engineering
[L2]
2. Students will learn the working concepts of Fixturing and various tools of
engineering [L2]
Program Outcome of this course (POs) PO No.
1. Graduates shall acquire in-depth knowledge in machine design and update the same,
integrating existing and updated knowledge in global perspective. [PO1]
2.
Graduates shall possess ability for independent judgment based on critical analysis
and also for synthesis of information for extensive research in the area of specialization.
[PO2]
3.
Graduates shall conceptualise through lateral thinking and obtain feasible and
optimal solutions for engineering problems considering societal and environmental
requirements.
[PO3]
Course delivery methods Assessment methods
1. Black Board Teaching 1. Internal Assessment
2. Power Point Presentation 2. Assignment
3. Working Models 3. Seminar
4. Videos 4. Mini-project
![Page 20: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/20.jpg)
Scheme of Continuous Internal Evaluation (CIE):
Components Average of best two IA
tests out of three
Average of
assignments (Two) / activity
Seminar/Mini
Project
Total
Marks
Maximum Marks: 50 30 10 10 50
Self Study topics shall be evaluated during CIE (Assignments and IA tests) and 10% weightage
shall be given in SEE question paper.
Scheme of Semester End Examination (SEE):
1. It will be conducted for 100 marks of 3 hours duration. It will be reduced to 50 marks for the
calculation of SGPA and CGPA.
2. Minimum marks required in SEE to pass: 20
3. Question paper contains 08 questions each carrying 20 marks. Students have to answer FIVE full
questions. SEE question paper will have two compulsory questions (any 2 units) and choice will
be given in the remaining three units.
![Page 21: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/21.jpg)
NON DESTRUCTIVE TESTING
Course Code CIM252 Credits 4
Course type PE CIE Marks 50 marks
Hours/week: L-T-P 4-0-0 SEE Marks 50 marks
Total Hours: 50 SEE Duration 3 Hours for 100 marks
Course learning objectives
1. The concept & need for inspection equipment and techniques. 2. The different methods of non destructive evaluation
Pre-requisites :Basic knowledge of Inspection techniques
Unit – I 10 Hours
Introduction to ND Testing: Visual Inspection, Laser Inspection, Coordinate Measuring Machine. Machine Vision and Robotic Evaluation. Leak Testing.
Self learning topics:Liquid Penetrant Inspection
Unit – II 10 Hours Magnetic Particle Inspection - Methods of generating magnetic field, types of magnetic particles and
suspension liquids steps in inspection.
Eddy Current Inspection- principles, operation variables, procedure, inspection coils, and detectable
discounts by the method
Self Learning Topics: application and limitations of magnetic particle inspection.
Unit – III 10 Hours
Microwave Inspection: Microwave holography, applications and limitations
Ultrasonic Inspection- Basic equipment characteristics of ultrasonic waves, variables inspection, inspection methods pulse echo A,B,C scans transmission, resonance techniques, search units, contact
types and immersion types inspection standards-standards reference books.
Self Learning Topics: transducer elements couplets
Unit – IV 10 Hours Acoustic Emission Inspection- relationship to other test methods, range and applicability, acoustic
emission waves and propagation, acoustic emission sensors and preamplifiers, instrumentation
principles, acoustic emission in material studies. Radiographic Inspection- principles, radiation source X-rays and gamma rays, X-ray-tube, radio
graphic films, neutron radiography, Thermal inspection principles, equipment inspection methods
applications.
Unit – V 10 Hours
Neutron Radiography- Principles of neutron radiography, attenuation of neutron beams, applications Optical Holography- Basics of Holography, recording and reconstruction - Acoustical Holography:
systems and techniques applications.
Self Learning Topics: neutron detection methods, Indian standards for NDT.
![Page 22: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/22.jpg)
Books
1. ASM Hand book , Non Destructive Evaluation and Quality Control – Vol 17, 2001. 2. Baldev Raj, T.Jayakumar . and M. Thavasimuthu, Practical Nondestructive Testing,
Narosa Publishing House, 2002
3. R.K .Jain, Engineering Metrology, Khanna Publishers, 1997 4. Progress in Acoustic Emission‟, Proceedings of 10th International Acoustic Emission
symposium, Japanese society for NDT,1990
5. Barry Hull and Vernon John, Non Destructive Testing, Macmillan, 1988
Course Outcome (COs)
At the end of the course, the student will be able to Bloom‟s
Level
1. Students will understand the concepts, techniques and applications of non
destructive testing [L2]
2. The students will describe the importance of non destructive testing in present
inspection world [L2]
3. The student will learn and explain the different types of different non destructive
methods [L2]
Program Outcome of this course (POs) PO No.
1. Graduates shall acquire in-depth knowledge in machine design and update the same, integrating existing and updated knowledge in global perspective.
[PO1]
2.
Graduates shall possess ability for independent judgment based on critical analysis
and also for synthesis of information for extensive research in the area of specialization.
[PO2]
3. Graduates shall be able to adopt modern techniques, analytical tools and softwares
for complex engineering solutions. [PO5]
Course delivery methods Assessment methods
1. Black Board Teaching 1. Internal Assessment
2. Power Point Presentation 2. Assignment
3. Working Models 3. Seminar
4. Videos 4. Mini-project
Scheme of Continuous Internal Evaluation (CIE):
Components Average of best two
IA tests out of three
Average of assignments (Two) /
activity
Seminar/Mini Project
Total
Marks
Maximum Marks: 50 30 10 10 50
Self Study topics shall be evaluated during CIE (Assignments and IA tests) and 10% weightage
shall be given in SEE question paper.
Scheme of Semester End Examination (SEE):
1. It will be conducted for 100 marks of 3 hours duration. It will be reduced to 50 marks for the
calculation of SGPA and CGPA.
2. Minimum marks required in SEE to pass: 20
![Page 23: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/23.jpg)
3. Question paper contains 08 questions each carrying 20 marks. Students have to answer FIVE full
questions. SEE question paper will have two compulsory questions (any 2 units) and choice will
be given in the remaining three units.
![Page 24: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/24.jpg)
ARTIFICIAL INTELLIGENCE AND EXPERT SYSTEMS
Course Code CIM253 Credits 4
Course type PE CIE Marks 50 marks
Hours/week: L-T-P 4-0-0 SEE Marks 50 marks
Total Hours: 50 SEE Duration 3 Hours for 100 marks
Course learning objectives
1. The course is aimed at providing a complete overview Artificial Intelligence and Expert System 2. The course is aimed in order to make the student aware of significance of AI & expert System‟s
application in advanced manufacturing applications
Prerequisites: Basic knowledge of control systems.
Unit - I 10 Hours
Human and Machine Intelligence; Concepts of fifth generation computing, programming AI environment, developing artificial intelligence system, definition of Expert systems, Natural
Language processing, neural networks.
Tools for Machine Thinking: Forward chaining, backward chaining, use of probability and
fuzzy logic.
Self Learning Topics: Functions of different parts of Mechatronic system
Unit - II 10 Hours
Expert System Development: Choice of Domain, collection of knowledge base, selection of
inference mechanism, case studies of expert system development in design and manufacturing. Advanced Programming Techniques: Fundamentals of object oriented programming, creating
structure and object, object operations, involving procedures, programming applications, object
oriented expert system.
Unit - III 10 Hours
Languages in AI: Using PROLOG to design expert systems, converting Rules to PROLOG, Conceptual example, introduction to LISP, Function evaluation, Lists, Predicates, Rule creation.
Unit - IV 10 Hours
Advanced knowledge representation for smart systems: Semantic nets-structure and objects,
ruled systems for semantic nets, certainly factors, Automated learning
Expert System Tools: General structure of an expert system shell, examples of creation of an expert system using an expert system tool.
Unit - V 10 Hours Industrial Application of AI and Expert systems: Robotic vision systems, Image processing
techniques, application to object recognition and inspection, automatic speech recognition.
Self learning topics: Robotic vision systems, Image processing techniques, application to object
recognition and inspection, automatic speech recognition.
![Page 25: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/25.jpg)
Books 1. Robert Levine et al, A Comprehensive guide to AI and Expert Systems, McGraw Hill Inc,
1986.
2. Henry C. Mishkoff, Understanding AI, BPB Publication, New Delhi, 1986.
Course Outcome (COs)
At the end of the course, the student will be able to Bloom‟s
Level
1. Familiarize and understand human and Machine Intelligence. [L2]
2. Understand tools for machine thinking and associated advanced programming
techniques. [L2, L3]
3. Demonstrate the application of AI & expert systems in industry [L3]
4. Explain fabrication, design and packaging of MEMS and Microsystems. [L1, L2]
Program Outcome of this course (POs) PO No.
1 Graduates shall possess ability for independent judgment based on critical analysis and also for synthesis of information for extensive research in the area of
specialization. [PO2]
2
Graduates shall conceptualise through lateral thinking and obtain feasible and
optimal solutions for engineering problems considering societal and environmental
requirements.
[PO3]
3 Graduates shall review relevant literature, apply appropriate research methodologies, working individually or as a team contributing to the advancement of domain
knowledge. [PO4]
4. Graduates shall be able to adopt modern techniques, analytical tools and softwares for complex engineering solutions.
[PO5]
Course delivery methods Assessment methods
1. Black Board Teaching 1. Internal Assessment
2. Power Point Presentation 2. Assignment
3. Working Models 3. Seminar
4. Videos 4. Mini-project
Scheme of Continuous Internal Evaluation (CIE):
Components Average of best two IA
tests out of three
Average of
assignments (Two) /
activity
Seminar/Mini
Project
Total Marks
Maximum Marks: 50 30 10 10 50
Self Study topics shall be evaluated during CIE (Assignments and IA tests) and 10% weightage
shall be given in SEE question paper.
![Page 26: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/26.jpg)
Scheme of Semester End Examination (SEE):
1. It will be conducted for 100 marks of 3 hours duration. It will be reduced to 50 marks for the
calculation of SGPA and CGPA.
2. Minimum marks required in SEE to pass: 20
3. Question paper contains 08 questions each carrying 20 marks. Students have to answer FIVE full
questions. SEE question paper will have two compulsory questions (any 2 units) and choice will
be given in the remaining three units.
![Page 27: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/27.jpg)
ADVANCED CONTROL ENGINEERING
Course Code CIM254 Credits 4
Course type PE CIE Marks 50 marks
Hours/week: L-T-P 4-0-0 SEE Marks 50 marks
Total Hours: 50 SEE Duration 3 Hours for 100 marks
Course learning objectives
1. To study various control techniques used in industrial automatic controls. 2. To study various frequency response methods. 3. To study various response and system compensation methods.
4. To get exposure of digital control systems
Pre-requisites: Should have knowledge of Basic Electronics and Control Engineering
Unit – I 10 Hours
Introduction to Automatic Controls: Steady-State Operation, Laplace Transforms. The Root-Locus Method: - Introduction, Root Locus Plots, Illustrations, General rules for
Constructing Root Loci, Root Locus Analysis of Control Systems, Transport Lag and Root contour
Plots.
Self Learning Topics: Representation of Control Components, Representation of Control
Systems, Characteristic functions.
Unit – II 10 Hours
Frequency Response Methods: - Introduction, Evaluating the Gain K, Equivalent Unity-Feedback Systems. Polar Plots, M And α Circles, Correlation between Transient and Frequency Response,
Determining the Gain K to Yield a Desired Mp, Relative Stability
Self Learning Topics: Frequency Response, Logarithmic Representation
Unit – III 10 Hours
System Compensation: Gain Margin and Phase Margin, Lead Compensation, Lag Compensation,
Lag-Lead Compensation.
Self Learning Topics: Nyquist Stability Criterion
Unit – IV 10 Hours State-Space Methods: - Introduction, Basic materials in State-Space Analysis, Transfer Matrices,
Controllability, Observability, System Representation, Signal Flow Graphs, Solution of State-Space
Equations, Transform Functions and Multivariable Systems.
Unit – V
10 Hours
Digital Control Systems: - Sampled-Data Systems, The Z Transform, Inverse Z Transforms, Block-
Diagram Algebra, Transient Response, Filters. Discrete Data Systems, Sampled-Data Control Systems, Computer-Controlled Systems
![Page 28: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/28.jpg)
Books
1. Francis H. Raven, Automatic Control Engineering, McGraw- Hill International, Third edition,
1978. 2. K. Ogata, Modern Control Engineering, PHI, Fifth edition, 2010.
3. B.C. Kuo, Automatic Control Systems, Prentice hall, Third edition, 1975. 4. Rao V. Dukkipati, MATLAB for Mechanical Engineers, 1st Edition, New Age International
Publishers, 2008
Course Outcome (COs)
At the end of the course, the student will be able to Bloom‟s
Level
1. Understand various control techniques used in modern engineering control system [L2, L3]
2. Understand various system compensation and response methods [L2, L3] 3. Explain digital control systems [L1]
Program Outcome of this course (POs) PO No.
1. Graduates shall acquire in-depth knowledge in machine design and update the same,
integrating existing and updated knowledge in global perspective. [PO1]
2.
Graduates shall conceptualise through lateral thinking and obtain feasible and
optimal solutions for engineering problems considering societal and environmental
requirements.
[PO3]
3.
Graduates shall possess ability for independent judgement based on critical analysis
and also for synthesis of information for extensive research in the area of
specialization. [PO4]
4. Graduates shall be able to engage in collaborative multidisciplinary scientific
research for decision making through rational analysis [PO6]
5 Graduate shall be able to introspect and apply corrections. [PO11]
Course delivery methods Assessment methods
1. Black Board Teaching 1. Internal Assessment
2. Power Point Presentation 2. Assignment
3. Working Models 3. Seminar
4. Videos 4. Mini-project
Scheme of Continuous Internal Evaluation (CIE):
Components Average of best two IA
tests out of three
Average of assignments (Two) /
activity
Seminar/Mini Project
Total
Marks
Maximum Marks: 50 30 10 10 50
Self Study topics shall be evaluated during CIE (Assignments and IA tests) and 10% weightage
shall be given in SEE question paper.
![Page 29: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/29.jpg)
Scheme of Semester End Examination (SEE):
1. It will be conducted for 100 marks of 3 hours duration. It will be reduced to 50 marks for the
calculation of SGPA and CGPA.
2. Minimum marks required in SEE to pass: 20
3. Question paper contains 08 questions each carrying 20 marks. Students have to answer FIVE full
questions. SEE question paper will have two compulsory questions (any 2 units) and choice will
be given in the remaining three units.
![Page 30: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/30.jpg)
RAPID PROTOTYPING AND CASTING ANALYSIS LAB
Course Code CIM26 Credits 2
Course type PC CIE Marks 25 marks
Hours/week: L-T-P 0-0-3 SEE Marks 25 marks
Total Hours: 30 SEE Duration 3 Hours for 50 marks
Course learning objectives
1. To enable the students to use CAD software for solid modeling 2. To enable the students to use RP process and parameters for prototyping 3. To enable the students to use Solidcast for casting analysis
List of experiments
1. Solid modeling using modelers like CATIA/SE of casting component 1 2. Solid modeling using modelers like CATIA/SE of casting component 2 3. Solid modeling using modelers like CATIA/SE of casting component 3 4. Rapid Prototyping system- introduction to FDM process and parameters
5. Making the RP parts for simple components 6. Introduction to Casting analysis, gating and riser design 7. Introduction to Solidcast- Casting parameters and process
8. Casting analysis of component using Solidcast, riser design parameters to predict
shrinkage. 9. Designing of riser, gates in modeling software.
10 Casting analysis of component incorporating riser and gates using Solidcast and
Flowcast to reduce shrinkage
Books 1. P.N. Rao, CAD/CAM Principles and Applications, McGraw Hill Education Pvt Ltd.,
3rd Edition, 2010. 2. Solidcast reference material, Finite Solutions Inc, 2015
3. Creatr (FDM) RP machine reference manual, Leapfrog, 2014. 4. P L Jain, Principles of Foundry Technology, Tata McGraw-Hill Education, Revised
edition, 2003.
Course Outcome (COs)
At the end of the course, the student will be able to Bloom‟s Level
1. Ability to understand the tools to model mechanical components. [L2]
2. Ability to understand the process to manufacture prototypes using FDM process [L2] 3. Ability to analyze castings for shrinkage and other defects.
[L4]
Program Outcome of this course (POs) PO No. 1. Graduates shall acquire in-depth knowledge in machine design and update the
same, integrating existing and updated knowledge in global perspective. [PO1]
2. Graduates shall be able to adopt modern techniques, analytical tools and [PO5]
![Page 31: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/31.jpg)
softwares for complex engineering solutions.
Assessment methods 1. Lab Internal Assessment
2. VIVA
Scheme of Continuous Internal Evaluation (CIE):
Components Conduct of the lab Journal submission Lab test Total Marks
Maximum Marks: 25 10 10 5 25
Submission and certification of lab journal is compulsory to qualify for SEE.
Minimum marks required to qualify for SEE : 13
Scheme of Semester End Examination (SEE):
1. It will be conducted for 50 marks of 3 hours duration. It will be reduced to 25 marks for the
calculation of SGPA and CGPA.
2. Minimum marks required in SEE to pass:
3.
Initial write up 2*10 = 20 marks
50 marks Conduct of experiments 2*10 = 20 marks
Viva- voce 10 marks
![Page 32: KARNATAK LAW SOCIETY‟S · 2017-01-17 · Self-Learning Topics: Casting Defects & Quality Control Casting defects: Shaping faults arising in pouring, Inclusions and sand defects,](https://reader030.fdocuments.in/reader030/viewer/2022040919/5e95813ee26d0c35466ed2e3/html5/thumbnails/32.jpg)
Bloom’s Taxonomy of Learning Objectives
Bloom‟s Taxonomy in its various forms represents the process of learning. It was developed
in 1956 by Benjamin Bloom and modified during the 1990‟s by a new group of cognitive
psychologists, led by Lorin Anderson (a former student of Bloom‟s) to make it relevant to the
21st century. The revised taxonomy given below emphasizes what a learner “Can Do”.
Lower order thinking skills (LOTS)
L1 Remembering Retrieve relevant knowledge from memory.
L2 Understanding Construct meaning from instructional material, including oral, written, and
graphic communication.
L3 Applying Carry out or use a procedure in a given situation – using learned
knowledge.
Higher order thinking skills (HOTS)
L4 Analyzing
Break down knowledge into its components and determine the relationships
of the components to one another and then how they relate to an overall
structure or task.
L5 Evaluating Make judgments based on criteria and standards, using previously learned
knowledge.
L6 Creating Combining or reorganizing elements to form a coherent or functional whole
or into a new pattern, structure or idea.