VANDEX CLADDING OF STONE/ BITUMINIOUS FELT.

Easy& Fast application (even when application (even when wet)wet)

No Protection needed (Cost saving).

Long Life Forms part of Structural concrete. Crack Bridge by crystallization

upto 0.3 mm . Sealmess and no fear of joint

failures due to age. Vandex Super is part and parcel of the structural concrete incase of structural alterations there are no cold joints formed due to age of applications.

Can be applied with ease from negative side of basement structure and can be applied post construction also.

Very Slow application and time consuming.

Protection needed (Extra cost) Extra cost of protection Does not form part of structure. Has very Limited crack bridging

capacity. Fear of Joint failure ever present

due to water pressure or age or poor workmanship

Does not form part of structural failure the system is not repairable from negetive side.

Can not be applied or used from negetive side or post construction.

Page 4: Fast basement waterproofing

BASEMENT TREATMENT

By: External Application Method

Page 5: Fast basement waterproofing

Typical Raft &Wall Joint Detail

Page 6: Fast basement waterproofing

Typical Detail Raft &Wall joint Typical Detail Raft &Wall joint

Page 7: Fast basement waterproofing

Method of Application:

SPRINKLING OF VANDEX SUPER JUST BEFORE CASTING OF RAFT

Doseage 1.0-1.2 Kg per Sq.mt

Quality.Control-Use of 1.0 Sq.mt Ring.

Page 8: Fast basement waterproofing

NEXT SEQUENCE

Page 9: Fast basement waterproofing

Correct Application ofCorrect Application of

Vandex ProductsVandex Products

Vandex International Ltd

Page 10: Fast basement waterproofing

Three elements of a successful

Vandex application

1. Surface preparation

Page 11: Fast basement waterproofing

How it shouldn’t be !!

• The laitance is still existing

Page 12: Fast basement waterproofing

Surface preparation

All concrete to be treated must be clean and have an ”open” capillary system. Remove laitance, dirt, grease, etc. by suitable means.

Page 13: Fast basement waterproofing

Concrete without any surface preparation

Page 14: Fast basement waterproofing

Concrete which received a surface preparation by high pressure water

jetting

• Aggregates are visible

Page 15: Fast basement waterproofing

Concrete which received a surface preparation by water-sandblasting

Page 16: Fast basement waterproofing

Water-sandblasting

• 180 bar water

• plus sand

Page 17: Fast basement waterproofing

Routing out visible cracks not subject to movements that exceed 0.3 mm

Crack repair

Page 18: Fast basement waterproofing

Repair of Retaining Wall

Page 19: Fast basement waterproofing

Cement based Injection Grouting

Page 20: Fast basement waterproofing

Three elements of a successful

Vandex application

1. Surface preparation

2. Product application

Page 21: Fast basement waterproofing

Application of Vandex products

Prewatering

Surfaces must be carefully prewatered prior to the Vandex application. The concrete surface must be damp but not wet.

Page 22: Fast basement waterproofing

Simple test by hand

Page 23: Fast basement waterproofing

Do not apply the products at temperatures below the values indicated on the product data sheet or on frozen substrates

Page 24: Fast basement waterproofing

Do not apply the products at temperatures below the values indicated on the product data sheet or on frozen substrates

Control of material consumption in relation to the surface => correct layer thickness

Page 25: Fast basement waterproofing

Do not apply the products at temperatures below the values indicated on the product data sheet or on frozen substrates

Control of material consumption in relation to the surface => correct layer thickness

When problems arise, stop the application and investigate => damage limitation

Page 26: Fast basement waterproofing

Do not apply the products at temperatures below the values indicated on the product data sheet or on frozen substrates

Control of material consumption in relation to the surface => correct layer thickness

When problems arise, stop the application and investigate => damage limitation

Record batch number of applied material

Page 27: Fast basement waterproofing

Mixing

Place in a clean container and stir for at least 3 minutes with a mechanical mixer.

Page 28: Fast basement waterproofing

Mixing

Place in a clean container and stir for at least 3 minutes with a mechanical mixer.

The mixing times have to be respected precisely !

Page 29: Fast basement waterproofing

Mixing

Place in a clean container and stir for at least 3 minutes with a mechanical mixer.

The mixing times have to be respected precisely !

The amount of water may – depending on environmental conditions and batch variations – differ slightly from the specified quantity.

Page 30: Fast basement waterproofing

Mixing

Place in a clean container and stir for at least 3 minutes with a mechanical mixer.

The mixing times have to be respected precisely !

The amount of water may – depending on environmental conditions and batch variations – differ slightly from the specified quantity.

If the mix stiffens, re-mix, do NOT add more water!

Page 31: Fast basement waterproofing

Mixing by mechanical mixer

Page 32: Fast basement waterproofing

Application by brush

• VANDEX SUPER

Page 33: Fast basement waterproofing

Curing

After application, Vandex treatments must be kept damp for 5 days.

Page 34: Fast basement waterproofing

Curing

After application, Vandex treatments must be kept damp for 5 days.