3
CP-HEAT.NL » FULL RENEWAL OF BOX COOLERS » IMPROVE COOLING CAPACITY » EXTEND BOX COOLERS’ SERVICE LIFE BOX COOLER PERFORMANCE PLAN

Transcript of BOX COOLER - CP Heat Exchanger

Page 1: BOX COOLER - CP Heat Exchanger

CP-HEAT.NL

» FULL RENEWAL OF BOX COOLERS

» IMPROVE COOLING CAPACITY

» EXTEND BOX COOLERS’ SERVICE LIFE

BOX COOLERPERFORMANCE PLAN

Page 2: BOX COOLER - CP Heat Exchanger

PRE-CLEANING TREATMENT At arrival in the workshop, the box cooler receives a pre-cleaning treatment in which the outer pollution will be removed. After pre-cleaning the cooler will be cleaned under high-pressure.

GRIT BLAST TREATMENT When the cleaning procedure is fully completed, the cooler is being grit blasted to get the best coating results.

CHEMICAL CLEANING TREATMENTThe box cooler goes in the chemical bath where the inner surfaces are rinsed. The last contamination will be removed during the high-pressure water jetting, after the chemical procedure is fi nished.

When your box cooler is fouled by marine growth (built-up algae or barnacles, for example), this ultimately affects its cooling capacity. CP Heat Exchanger Technologies developed a program to renew your box cooler and restore its performance. Within this program the box cooler will be treated with a special cleaning method, a grit blast treatment and multiple layers of coating will be applied. Optionally we can overhaul your box cooler or perform repairs. This renewal program ensures a complete restore of the cooling capacity and bring your box cooler back to its maximum performance.

ULTIMATE PROTECTION: PHENOL COATING & ANTI-FOULINGWithin the box cooler performance plan the cooler will be treated with three layers of phenol coating. This coating protects the cooler against corrosion. Additional, an extra layer of anti-fouling can be applied. The antifouling coating minimizes accretation of marine organisms and is therefore perfectly suitable for vessels that sail in shallow, warm waters at lower speeds. A combination of both type of coatings will give your cooler the ultimate protection.

BOX COOLERPERFORMANCE PLAN

BOX COOLER RENEWAL TREATMENT

COATINGAfter grit blasting, a special phenol coating will be applied. This coating slows down the accretation of marine organisms as far as possible and helps protect the box cooler against the corrosive effects of seawater.

Specialist in total refurbishment ofheat exchangers.

MAINTENANCE & REPAIRIf desired, we can also overhaul your box cooler.

The following works will be performed:• disassembly, cleaning and assembly of covers • installation of new gaskets • replacement of nuts and bolts • application of a new coat of paint to the covers • threading and wire-brushing of tube plates • pressure testing

Additional we can also replace damaged tubes (retubing).

Page 3: BOX COOLER - CP Heat Exchanger

CP HEAT EXCHANGER TECHNOLOGIES B.V.Jan van Galenstraat 86, 3115 JG SchiedamT +31 (0) 10 429 61 04E [email protected]

CP-HEAT.NL