Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September...

11
Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009

Transcript of Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September...

Page 1: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009.

Atomic Layer Depositionfor Microchannel Plates

Jeffrey Elam

Argonne National Laboratory

September 24, 2009

Page 2: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009.

Atomic Layer Deposition (ALD)

Layer-by-layer thin film coating method Atomic level control over thickness and composition Precise coatings on 3-D objects Deposit nearly any material (oxides, nitrides, metals, etc.)

Example:ALD Zinc Oxide in

deep trenches

Page 3: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009.

Large Area Photodetector

Microchannel Plate (MCP)

– Electron amplifier (x104-107)

3

Page 4: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009.

Microchannel Plates (MCPs)

Conventional Fabrication:– Draw glass fiber bundle– Slice and polish– Chemical etch, heat in hydrogen

Problems:– Expensive– Resistance and secondary emission properties are linked– Long conditioning process needed– Thermal runaway

4

Page 5: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009.

ALD for Fabrication of MCPs

Start with porous, insulating substrate

– Glass capillary plate

– Anodic aluminum oxide (AAO) membrane ALD of resistive film on all surfaces (inside of pores, on faces, etc.) ALD of secondary electron emissive film Deposit metal electrodes on outer surfaces

5

33 mm

Page 6: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009.

MCP Structure

6

1) resistive coating (ALD)2) emissive coating (ALD)3) conductive coating (thermal

evaporation or sputtering)

pore

Page 7: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009.

ALD for Resistive Coating

Target: 10-100 MΩ through MCP ZnO: conductor Al2O3: insulator

ZnO/ Al2O3 alloy – tunable resistivity

Tune composition and thickness of film to adjust MCP resistance

7

Page 8: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009.

ALD for Emissive Coating

8

Many material possibilities Tune SEE along pore

SiO2Al2O3

MgO

ZnO

Page 9: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009.

Cross-Sectional Elemental Maps of ALD MCP

9

Zn

SEM Si

Al Au

ALD ZnO and Al2O3 extend into pores

Sputtered Au only on edge of pores

Glass capillary plate ALD ZnO/Al2O3

Sputter gold electrodes

Page 10: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009.

Cross-Sectional Image of ALD Film in MCP

10

ALD Film

100 nm ALD film visible in middle of MCP

Glass

Page 11: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009.

Questions?

11