EvisiveScan - National Physical...

Post on 06-Mar-2018

215 views 1 download

Transcript of EvisiveScan - National Physical...

EvisiveScanTM

Microwave Scanning NDT

Bob Stakenborghs

Evisive General Manager

Level III MW NDT

Microwave Definition

Evisive 2

Frequencies: 1.6-30 GHz

Wavelengths: 187 - 10 mm

Microwave inspection Principles of Operation

• Material under inspection is bathed in MW energy of an essentially constant frequency creating a series of standing waves in the object

Evisive 3

Principles of Operation

Evisive 4

The boundary in this case is any change in relative permitivity (Commonly known as Dielctric Constant) o f the material.

Energy is reflected from each interface of differing relative permitivity within specimen

Measurement Technique

Evisive 5

B A

Transmitter

¼ λ

The reflected energy is measured and creates a resulting output voltage signal

Data Collection

Evisive 6

The resulting voltage is sampled at discreet locations across sample to create an image

Image Creation

Evisive 7

MW Inspection Overview

• Multiple generations of equipment in the field

• Mechanical inspection devices for:

– HDPE butt fusion and electrofusion joints

– HDPE, FRP pipes and vessels (up to 12 feet in diameter)

– Rubber expansion joints

– Fully battery operated and bluetooth data transfer inspection equipment

• Microwave Inspection accepted as a new technique in ASNT

• ASTM Standards under development

• Microwave represented in ASME BPVC working groups on HDPE

Evisive 8

Detectable Defect Types

• Disbonds & Lack of Fusion in HDPE Butt Fusion and Electrofusion Thermal Welds

• Foreign Material Inclusions

• Voids

• Moisture or other liquid contamination

• Mechanical damage

• Physical changes due to chemical attack

Evisive 9

Current Uses

• Fiberglass Tanks and Pipes • Dow • Bayer • Borouge • Shell

• Fiberglass Armor • US Army (SBIR) • Kazak

• Reinforced Rubber Expansion Joints • Exelon • PSEG • FENOC • Wolf Creek

• Ceramic Materials • US Air Force (SBIR)

• HDPE Butt Fusion Joints • Axiall

Evisive 10

Work In Progress

• Enhanced imaging techniques using Narrow Band Synthetic Aperture Focusing Techniques (SAFT)

– Allow specific depth location

Transition to Wide Band SAFT

– Provide for 3D imaging (holographic) techniques

Evisive 11

FIRST GENERATION LAB EQUIPMENT

EvisiveScanTM

Microwave Scanning NDT

Evisive 12

Basic Equipment Setup Laboratory Scan Table

Laboratory Scan Lathe

Evisive 13

NEW GENERATION FIELD EQUIPMENT

EvisiveScanTM

Microwave Scanning NDT

Evisive 14

Blue Tooth Hand Held

Evisive 15

Evisive 16

Pipe Scanner

Pipe with manufactured defects

Pipe with erosion defects and insufficient glue Inspection image of pipe

17

Pipe with manufactured defects

Gray scale image showing interference pattern at erosion hole 3D rendering of pipe

18

3D Rotated view of part

19

Fiberglass Panel

20

Thickness determination

21

MICROWAVE INSPECTION OF GFR

22

EVISIVESCANTM

MICROWAVE SCANNING NDT

Overloaded section of fiberglass boom

Boom section Inspection image

23

Delamination

Internal erosion of pipe

24

Displaced structure caused by washout of resin matrix

Localized Pit

Voiding at manufacture

Boom with voiding Inspection image of boom

25

Voiding identified in inspection image

Internal pipe hydrolysis

Picture of pipe ID Inspection image of pipe ID

26

Internal blistering identified in image

Environmental degradation of furan pipe

Photo showing chemical attack Inspection image of chemical attack

27

Degraded resin to right of line

Resin poor areas of pultruded panel

28

A 1816

B 1217

C 1597

D 1114

Tensile test results (Pounds load to failure)

Panel with various types of fod

29

Image focus changes based on relative position of the end of the antenna with respect to the material surface

Metal, paper, cloth FOD

INSPECTION OF STEEL PIPE CORROSION BENEATH FIBERGLASS OVERWRAP

EVISIVESCANTM

MICROWAVE SCANNING NDT

Corrosion Beneath Fiberglass Overwrap

Figure 1-Corrosion under fiberglass overwrap

• In service inspection of steel pipe corrosion under insulation or overwraps.

• Condition monitoring of pipe over time

The wrap is hard fiber reinforced layer with

mastic matrix and interlayer fill.

Scan image shows features in pipe surface, at

pipe to wrap interface and in pipe wrap.

Indications inclued artificial and unintended

features.

Pipe Wrap with Artificial Defects

Pipe wrap with artificial defects. The wrap is flexible fiber material with a resin matrix. Microwave interference scan of pipe wrap showing features in pipe surface, at pipe to interface and in pipe wrap volume. Indications include artificial and unintended features.

Pipe Wrap with Artificial Defects

Outside end Inside end

Outside

end again

circumference

Good bond / whole area

Clockspring Inspection

Crack

Strong indication, likely disbond at metal surface

Section at

x = 8 in.

Clockspring inspection

Good Bond

Section at

x = 18 in.

Clockspring inspection

Corrosion/

Delamination at pipe surface

Section at

x = 29 in.

Clockspring inspection

THICKNESS MEASUREMENT

Evisive 38

EVISIVESCANTM

MICROWAVE SCANNING NDT

Thickness Measurement

Evisive 39

B

A

Transm

itter

¼ λ

0

-2

B

A

Transm

itter

¼ λ

+

2

-1

B

A

Transm

itter

¼ λ

+

0

+

1

Phase Plot

-1.5

-1

-0.5

0

0.5

1

1.5

-1.5 -1 -0.5 0 0.5 1 1.5

Ch

B

Ch A

Evisive 40

Calibration Panel

Evisive 41

Phase & Magnitude Application

Evisive 42

Wedge used to correlate thickness to color

Thicker area

Area with wall loss

Wall loss = .150”

Wall Loss=.050”

Wall Loss = .155”

Wall Loss = .060”

Fiberglass Panel

Evisive 43

Inspection Image

Evisive 44

3D Representation

Evisive 45

Evisive 46

QUESTIONS?

EvisiveScanTM

Microwave Scanning NDT